SHF 333

Standards

EN ISO 14174 S A FB 3
TS EN ISO 14174 S A FB 3

Properties and Applications

Alloyed and agglomerated flux, which is designed for submerged arc hardfacing of parts subjected to metal to metal friction wear, moderate impart and low stress mineral abrasion. Provides weld metal with 300-350 HB hardness, when used with SW 702 wire electrode. Possible to use in direct current. Hardness and transfer of alloying elements to the weld metal depens on welding parameters used. Gives very smooth and clean weld bead surfaces, slag removal is very easy and generally slag is self releasing.

Typical Applications : Hardfacing of track rollers, idlers, couplings, piston rod ends, earth moving equipment, rolls, mills, etc. the alloying effect to the flux depends, to a large degree, on the weld parameters chosen.
Shf 333 Sert Dolgu

Wear Resistance Types


Abrasion

Adhesion

Impact

Temperature

Corrosion
Low
Medium
High
Very High

Typical Applications

Shf 333 Model Tipik Uygulamalar Shf 333 Model Tipik Uygulamalar Shf 333 Model Tipik Uygulamalar Shf 333 Model Tipik Uygulamalar

Typical Chemical Values of Weld Metal

Welding WireType of AnalysisCSiMnCrMo
SW 702Weld Deposit0.151.001.302.500.45

Typical Mechanical Values of Weld Metal(%)

Test ConditionWelding WireHardness (HB)Hardness (HRc)
As weldedSW 702300 - 35032 - 35

Application Information

Welding Positions :
Shf 333 Kaynak Pozisyonu Shf 333 Kaynak Pozisyonu

Polarity:

Shf 333 Kutuplama DC(+)

Welding Parameters & Efficiency :

Packaging Information

Product CodeWeight Of The Box (kg)Number Of Boxes Per PackageWeight Of The PackagePackaging Type
408030AGM225.0125.6Kraft Bag

Storage & Re-Drying Information

>The total drying duration should not exceed 10 hours ( also for repeated drying).
>During transportation and storage, it should be ensured that the packaging is not damaged or torn.
>It has to be dried at 350°C for 2 hours.